SHANON CLUB PLYWOOD

190.00

100% Red Core | 710-Marine | WBP Grade

Melamine Fortified Resin
Termite & Borer Resistant
Bend & Warp resistant
Reduced Water absorption
Gurjan Face Veneer

Category:
Description

Shanon Club Plywood is made from 100% Red Core veneers bonded with undiluted phenol-fortified resin using pre-press technology to make it boiling waterproof. Shanon Club Plywood is built to withstand the elements whether it be frequent humidity variations or harsh conditions, Shanon Club Plywood stands the test of time.

Shanon Club Series plywood is composed using only 8×2 feet full core panels, which ensures zero gaps, zero overlapping, zero warp or bending as well as strong nailing and screwing capability without splitting. Conforms to IS: 710: Marine which means Shanon Club ply can withstand 72 hours soaking in boiling water without missing a beat. The Shanon Club series is built to last a lifetime.

Applications :

Boats, Heat Exchangers, Sign Boards, Marine and River Crafts, Public Hoardings, Roofing & other exposed outdoor structures.

Technical Information :

Glue Shear Strength Dry State                 1350 N Avg. 1100 N Min. Individual Avg.
Glue Shear Strength Wet State                1000 N Avg. 800 N Min. Individual Avg
Screw Holding Strength (Kg)                     250
Specific Gravity                                           750 kgs/Cubic Meter
Nail Holding Strength (Kg)                         60
Modulus Of Rupture                                   400 Kgs/cm2

Tensile Strength :

Parallel To Grain Direction                          425 KN/m2
Perpendicular To Grain Direction              250 KN/m2
Sum In Both Directions Minimum             850 KN/m2
Stands 72 hours soaking at 100°C
Conforms to IS 710 – 1976